...floating on the ocean surface and in the intertidal zone. Polyethylene (PE) and polystyrene (PS) of two different sizes (10 and 100 µm) were weathered in rotating seawater for 80 days under two different conditions: (1) photodegradation equivalent to ≤616 average days in Trondheim and (2) mechanical degradation...