The influence of Ca2+ in de-icing salt on the chemistry of corrosion products formed on AM50 magnesium alloy – calcareous deposition

Sammendrag

The corrosion inhibiting effect of Ca2+ – which was presented in a previous publication of the authors [1] under immersion conditions in the first 4.5 h – cannot be attributed to the incorporation of Ca2+ into the surface layer as demonstrated by EDX and XPS measurements. XPS depth profiling indicates that an increase of the corrosion product layer thickness and a higher amount of more protective magnesium carbonates in the outmost surface layer seem to be responsible for the inhibiting effect in presence of Ca2+. Furthermore, the corrosion products formed in presence of Ca2+ exhibit less incorporation of water and hydroxyl species under short time immersion conditions, as shown by FTIR-measurements.
After several days of immersion in the presence of Ca2+ in the solution a white, open-porous deposition covers the sample surface and the element Ca could be detected on the surface by EDX analysis. XRD and FTIR measurements proved the presence of calcite, with layer thicknesses up to 155 µm, shown by SEM investigations. The alkalization of the electrolyte during magnesium alloy corrosion and the presence of Mg2+ trigger the deposition of an intermediate deposition product CaMg(CO3)2 which transforms to CaCO3 under conditions of low CO2 partial pressure.

Kategori

Vitenskapelig artikkel

Språk

Engelsk

Forfatter(e)

Institusjon(er)

  • Tyskland
  • Friedrich-Alexander-Universität Erlangen-Nürnberg
  • SINTEF Industri / Materialer og nanoteknologi

År

2015

Publisert i

Corrosion

ISSN

0010-9312

Forlag

NACE International

Årgang

71

Hefte nr.

6

Side(r)

703 - 725