DSC – Differential Scanning Calorimeter – with high pressure cell
Kontaktperson
Manufacturer: Mettler Toledo
Differential Scanning Calorimeter with high pressure cell making measurements possible from 1 to 100 atm in oxygen or nitrogen atmosphere.
- Temperature range: RT to 700 C.
- Sensor resolution < 0.04 µW
- Water cooling available.