Freezing dilatometry on concrete with varying ASR at different degrees of saturation

Abstract

Freezing dilation clear function of DS/DCS: DScrit ≈ 0.80 in ASR affected concrete from Voll • Hydraulic pressure induced expansion observed at DS = 0.86 and 0.90, i.e. frost damage mainly occurs during temperature drop, and less at constant low temperature. • At DS = 0.86 «some growth of bodies of ice» observed • All concrete specimens are presumably non-air entrained, hence pre-existing cracks will accelerate damage (Zhou, Cohen & Dolch ACI 1994) • The effect of pre-existing cracks by ASR in frost-degradation of Non-Air entrained concrete: – Deterioration as surface scaling inside water filled cracks – high DS - (photo slides 13-14), presumably by HP due to high DS – If crack is not water filled (vertical part of structure, crack to wide to suck water) and DS < DScrit then crack widening over time is due to ASR (due to expanding core concrete?)

Category

Other presentation

Language

English

Author(s)

Affiliation

  • SINTEF Community / Infrastructure
  • Norwegian University of Science and Technology

Presented at

FACILE-CPR, CEN/TC 51/WG 12/TG 4 & NORDIC CONCRETE FEDERATION joint Workshop October 29th-30th 2026 on “Optional essential Characteristics” Differentiated testing methodology/-ies to accommodate for diversified climatic exposure and concrete material response and performance.

Place

SINTEF Trondheim, ZEB Laboratory, 3rd floor, Høgskoleringen 13, Trondheim

Date

29.10.2026 - 30.10.2026

Organizer

SINTEF

Year

2026

View this publication at Norwegian Research Information Repository